Ways to avoid quenching cracks
Source: China Bearing Network Time: 2013-04-05
/*250*250 was created on 2017/12/25*/ var cpro_id = 'u3171089'; |
1. The correct depiction of the product should be based on the working conditions of the product (the type of force and the size of the big dew 鹊 鹊 å© èŠªÐ£ 芪У 龋 龋 龋 龋 龋 龋 龋 æ…µ æ…µ æ…µ æ…µ æ…µ æ…µ æ…µ æ…µ æ…µ æ…µ æ…µ æ…µ æ…µ æ…µ æ…µ æ…µ æ…µShepherd 缓 æ·¼ æ·¼ æ·¼ æ·¼ æ·¼ æ·¼ 岢鋈 岢鋈 岢鋈 岢鋈 岢鋈 岢鋈 岢鋈 岢鋈 岢鋈 ç ¸ ç ¸ ç ¸ ç ¸ ç ¸ ç ¸ ç ¸ ç ¸
2. Reasonable arrangement of process lines When the data, layout and skill conditions of the parts are determined; the process personnel should carry out process analysis; determine the reasonable process lines. Properly arrange the orientations of the preparation heat treatment, ice face processing and thermal processing. This is a useful way to improve product quality, improve efficiency, and avoid the tendency of heat treatment to crack.
3, properly determine the heating parameters in the heat treatment production; improper heating is the main factor leading to quenching cracking. Therefore; heating parameters such as heating medium, heating rate, heating temperature and holding time; should be correctly selected and depicted.
4. Selecting a reasonable quenching method depends on the layout and characteristics of the parts and skill requirements; the correct and reasonable selection of quenching methods such as the layout and the nature of the workers can greatly reduce or eliminate the quenching.
5. Selection of quenching medium The selection of quenching medium should be summarized into the following elements:
Part characteristics: the chemical composition of the steel (phase change characteristics); the cross-sectional dimension of the workpiece; several shapes; the appearance roughness and appearance; the placement and density of the parts during quenching.
Quenching method: including quenching bath, mixing speed, flow direction, concentration of solution.
6. Other methods to avoid quenching cracks Temporarily temper after quenching; partial dressing of thin-walled parts with disordered shapes can also be used to avoid cracks.
Recommend to friends comments close window
Bearing related knowledge |
Inch Tapered Roller Bearing LM102949/10 Jiuzhou eight types of bearing distribution department skills support: thrust ball bearing composition layout pitch bearing fretting wear analysis of rolling bearing clearance measurement skills (a) How to remove the motor bearing |
This article links to http://
Please indicate the bearing network http://
Previous: SKF Bearing Active Self-aligning Ball Bearing Performance and Features Next: Jiang Drilling Successful Metal Bearing Sealing Drill
For sea-water shrimp, fish, eel & crab: 1.0-2.0 KG/Ton complete feed
For fresh-water shrimp & Fish: 1.0-1.5 KG/Ton complete feed
Those Aquatic attratant products can be added to premix, concentrates, etc. As feed intake, the range is not limited to fish feed, including bait. This product can be added directly or indirectly, as long as the attractant and feed can be mixed well.
Widely use
Aquatic Attractant,Feed Grade Trimethylamine Chlorhydrate,Trimethylamine Oxide Dihydrate,Dmt Aquatic Attractant
SHANDONG E.FINE PHARMACY CO., LTD , http://www.sdefine.com